Fire Sci. Eng. Search

CLOSE


Fire Sci. Eng. > Volume 31(2); 2017 > Article
Fire Science and Engineering 2017;31(2):37-43.
DOI: https://doi.org/10.7731/KIFSE.2017.31.2.037    Published online April 30, 2017.
생활 주변에서 사용되는 건축용 목재의 연소성
우태영, 유지선, 정영진
1강원대학교 방재전문대학원
2강원대학교 방재전문대학원
3강원대학교 소방방재공학과
Combustion Properties of Construction Lumber Used in Everyday Life
Woo Tae-young, You Jisun, Chung Yeong-jin
1Graduate School of Disaster Prventoion, Kangwon National University
2Graduate School of Disaster Prventoion, Kangwon National University
3Dept. of Fire Protecton Engineering, Kangwon National University
요약
이 연구에서는 4종의 삼나무, 스프러스, 나왕, 레드파인 시험편을 콘칼로리미터(Cone calorimeter, ISO 5660-1, 2)와 연기밀도시험기(ASTM E 662)를 이용하여 연소성을 시험하였다. 그 결과, 삼나무가 착화시간이 가장 빨랐고 평균열방출율($HRR_{mean}$)이 $58.52kW/m^2$으로 가장 낮게 나타났다. 그리고 레드파인의 평균열방출율($HRR_{mean}$)이 $71.75kW/m^2$으로 가장 높게 나타났다. CO 발생량에서는 나왕과 삼나무가 가장 많이 발생하였고, 반대로 $CO_2$ 발생량에서는 레드파인과 스프러스가 가장 많이 발생하였다. 동적방법에서의 총연기방출율은 레드파인이 연기가 가장 많이 발생하였고, 스프러스가 가장 적게 발생하였다. 정적방법에서의 연기밀도는 레드파인이 훈소(Non-flaming) 방식과 불꽃(Flaming) 방식에서 가장 높았다. 나왕은 훈소(Non-flaming) 방식에서 2번째로 연기가 많이 발생한 데 반하여 불꽃(Flaming) 방식에서는 가장 적게 발생한 것을 알 수 있었다. 열방출율 측면에서 화재위험성은 4가지 시험편 중 레드파인이 가장 높았다. 연기발생 관점으로 보아도 동적인 방식과 정적인 방식 모두 레드파인이 화재 위험성이 가장 높은 재료였다.
Abstract
The combustion characteristics of four kinds of wood specimens, such as Japan cedar, spruce, lauan, and red pine, were tested using the standards of Cone calorimeter (ISO 5660-1, 2) and smoke density tester (ASTM E 662). Japan cedar caught fire the quickest but the mean heat release rate was the lowest, $58.52kW/m^2$. The mean heat release rate of red pine appeared to be the highest, $71.75kW/m^2$. The lauan and Japan cedar generated relatively large amounts of carbon monoxide while the red pine and the spruce generated relatively large amounts of carbon dioxide. The red pine generated large amounts of smoke and the spruce generated the least amounts of smoke than the other samples. The total smoke release rate in the dynamic method was the highest in red pine and the lowest in spruce. The smoke density of red pine in the static method was highest in the non-flaming and flaming methods. In the non-flaming method, the smoke density of lauan was the second highest, whereas the flaming method was the least. In terms of the heat release rate, the fire risk from red pine was highest among the four test specimens. From the viewpoint of smoke generation, red pine was the most dangerous material in both dynamic and static methods.
Key Words: Cone Calorimeter (ISO 5660-1,2), Combustion Properties, Smoke, Smoke Density Tester (ASTM E 662)


ABOUT
BROWSE ARTICLES
EDITORIAL POLICY
AUTHOR INFORMATION
Editorial Office
Room 906, The Korea Science Technology Center The first building, 22, Teheran-ro 7 Gil, Gangnam-gu, Seoul, Republic of Korea
Tel: +82-2-555-2450/+82-2-555-2452    Fax: +82-2-3453-5855    E-mail: kifse@hanmail.net                

Copyright © 2024 by Korean Institute of Fire Science and Engineering.

Developed in M2PI

Close layer
prev next